Oil pan
Before
Tool |
Wire brush |
---|---|
Problem |
Scratches are left by deburring with wire brushes. |
After
Tool | XEBEC Brush™ Surface |
---|---|
Result | Full automation deburring with machining center realized with improved surface quality. |
Workpiece information
Industry |
Automotive |
---|---|
Part name |
Oil pan |
Material type |
Alminium alloy |
Machining process |
Front cutter processing |
Industry |
Automotive |
---|---|
Part name |
Camshaft |
Material type |
FCD |
Machining process |
Drilling |
Processing conditions
Tool | XEBEC Brush for Surface (A31-CB25M) |
---|---|
Details of processing | Deburring of the matching surface after face milling process. |
Spindle speed (min⁻¹) | 2000 |
Table feed (mm/min) | 3000 |
Depth of cut (mm) | 0.5 |
Machining time (sec) | – |