Plate
Before
Tool |
Plastic brush |
---|---|
Problem |
The brush edge deformed. The inner diameter of cross hole H7 could not be maintained. Mass production machining was not possible. |
After
Tool | XEBEC Brush for Surface (A11-CB60M) |
---|---|
Result | Deburring with maintaining the inner edge profile of cross hole H7 without deformation realized. Quality requirement achieved. Also, tool life 65000 pcs/brush realized. |
Workpiece information
Industry |
Automotive |
---|---|
Part name |
Plate |
Material type |
SPH440 |
Cutting process |
Others |
Processing conditions
Tool |
XEBEC Brush for Surface (A11-CB60M) |
---|---|
Details of processing |
Deburring the external circumference edge and (4) bores. |
Spindle speed (min⁻¹) |
900 |
Table feed (mm/min) |
– |
Depth of cut (mm) |
1 |
Machining time (sec) |
3 sec |