Wing rib
Before
Tool |
Belt sander |
---|---|
Problem |
It took time for deburring due to large workpiece. |
After
Tool | |
---|---|
Result |
By the introduction of automated deburring, stable quality realized in a shorter cycle time. |
Workpiece information
Industry |
Aerospace |
---|---|
Part name |
Wing rib |
Material type |
Aluminum |
Cutting process |
End mill processing |
Processing conditions
Tool |
XEBEC Brush Surface (A11-CB25M) |
---|---|
Details of processing |
Deburring after end milling process |
Spindle speed (min⁻¹) |
4,000 |
Table feed (mm/min) |
800 |
Depth of cut (mm) |
0.7 |
Machining time (sec) |
– |